| PP-R RP2400 韩国大韩油化工业公司 物性数据 |
| 暂无此原料描述部分┄ |
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | |
| 基本性能 | 熔体流动速率 | --- | ASTM D-1238 | 0.25 | g/10min |
| 密度 | --- | ASTM D-1505 | 0.9 | g/cm3 | |
| OIT | 200℃ | ASTM D-3895 | >30 | min | |
| 吸水性 | --- | ASTM D-570 | >0.01 | % | |
| 机械性能 | 屈服拉伸强度 | --- | ASTM D-638 | 230 | kgf/cm2 |
| 断裂伸长率 | --- | ASTM D-638 | >600 | % | |
| 弯曲模量 | --- | ASTM D-790 | 8500 | kgf/cm2 | |
| 洛氏硬度 | --- | ASTM D-785 | 72 | R Scale | |
| 艾佐德冲击强度 | Non-Notched | ASTM D-256 | NB | kgfcm/cm | |
| 艾佐德冲击强度 | Notched,23℃ | ASTM D-256 | 60 | kgfcm/cm | |
| 电气性能 | 体积电阻率 | --- | ASTM D-257 | 1 | 1017Ω.H |
| 介电常数 | 1KHz | ASTM D-150 | 2.3 | --- | |
| 耗散(损耗)因数 | 1KHz | ASTM D-150 | 2 | 10-4/℃|10-4/℃ | |
| 介电强度(短时间) | --- | ASTM D-149 | 40 | KV/М | |
| Arc Resistance | --- | ASTM D-495 | 130 | sec | |
| 热 性 能 | 热传导性 | --- | KPIC Method | 3 | 10-4calcm/cmsec℃ |
| 热变形温度 | --- | ASTM D-648 | 85 | ℃ | |
| 比热性 | --- | ASTM D-648 | 0.46 | Ш/g℃ | |
| 熔点 | --- | ASTM D-3418 | 139 | ℃ | |
| 维卡软化点 | --- | ASTM D-1525 | 133 | ℃ | |