| PPS A504X90 日本东丽工业株式会社 物性数据 |
| 规格级别: | 玻璃纤维增强级 | 外观颜色: | --- |
| 用途概述: | --- | ||
| 备注说明: | 特性:高抗冲击,高韧 | ||
| 性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||||||||||
| 基本性能 | 吸水率 | 24hr,23℃于水中 | ASTM D-570 | 0.02 | % | |||||||||
| 物理性能 | 比重 | --- | ASTM D-792 | 1.67 | --- | |||||||||
| 泰伯磨耗 | --- | ASTM D-D1044 | 50 | mg/1000次 | ||||||||||
| 摩擦系数/对铁 | --- | ASTM D-1894 | 0.25 | --- | ||||||||||
| 限定PV值 | --- | TORAY | 815 | kj/m2.hr | ||||||||||
|
--- |
|
|
|
||||||||||
| 机械性能 | 洛氏硬度 | --- | ASTM D-785 | 122 | R | |||||||||
| 拉伸强度 | 23℃ | ASTM D-638 | 207 | Mpa | ||||||||||
| 延伸率 | 23℃ | ASTM D-638 | 3.6 | % | ||||||||||
| 弯曲强度 | 23℃ | ASTM D-790 | 275 | Mpa | ||||||||||
| 弯曲模量 | 23℃ | ASTM D-790 | 13.3 | GPa | ||||||||||
| 压缩强度 | --- | ASTM D-732 | 80 | --- | ||||||||||
|
--- |
|
|
|
||||||||||
| 电气性能 | 阻燃性 | --- | --- | V-0 | UL94 | |||||||||
| 抗电弧性 | --- | ASTM D-495 | 127 | Second | ||||||||||
| 体积电阻 | --- | ASTM D-257 | 1016 | Ω.m | ||||||||||
| 介电强度 | --- | ASTM D-149 | 21 | MV/m | ||||||||||
| 介电常数 | 106Hz | ASTM D-150 | 3.8 | --- | ||||||||||
| 损耗因子 | 106Hz | ASTM D-150 | 0.002 | --- | ||||||||||
| 热 性 能 |
|
--- |
|
|
|
|||||||||
| 熔点 | --- | DSC | 278 | ℃ | ||||||||||
| 热变形温度 | 1.82MPa | ASTM D-648 | >260 | ℃ | ||||||||||
| 其它性能 | 流动长 | 320℃,98MPa | TORAY | 100 | ×10-3m | |||||||||